Technology & Chemical Composition

Maske FFP2

With the help of advanced technology, steel is produced through the DRI-EAF route while the production process is being taken place at Integrated Steel Plant ……. The final billets are rolled into TMT Re- bars with different sizes and standardized grades. In the Sponge iron plant iron-ore, coal and dolomite will get charged.The reaction between carbon in coal and oxides in iron-ore, iron-ore transforms into Sponge iron.

The procedures involved in an arc furnace are as follows:

Charging

Melting

Refining

De-slagging

Tapping



APOLLO TMT-Chemical Composition
BIS % APOLLO %
Carbon 0.30 0.20 – 0.30
Manganese 0.30 – 0.60 0.50 – 0.70
Sulphur 0.06 0.055
Phosphorus 0.06 0.055
Bend Properties of APOLLO Fe-500 EQR
Test IS 1786 Fe 500
Bend 30 up to 20 mm, 40 over 20 mm
Rebend 50 up to 10 mm, 70 over 10 mm
Corrosion Resistant - APOLLO Fe-500 EQR
Test IS 1786 Fe 500
Copper + Chromium + Phosphrus 0.50 min %